How do you specify an MS sealant for a wet-area joint?
This case splits a wet area into two joints. A kitchen or bathroom joint asks for MS973-KB, the grade named for mould resistance. A balcony edge is on this page only when it is a low-movement wall joint, and that joint stays on universal grade MS973. Neither joint is a coating over the slab. This page does not name a customer.
Which grade
| Joint | What to ask for |
|---|---|
| Kitchen or bathroom | MS973-KB, named for mould resistance. The published density, tack-free time and tensile strength belong to MS973. They are not copied onto MS973-KB until that grade has its own sheet. |
| Balcony edge | Use MS973 only when the joint is a low-movement wall joint on the MS973 sheet. Keep the width-to-depth ratio at 2:1. This is not a membrane over the balcony. |
| Natural stone | Run a stain test on an off-cut before the job. The sheet asks for a compatibility test when the substrate is not confirmed. |
| Paint | If the joint will be painted, use water-based paint after cure and test that coating first. |
| Closed void | Do not use the sealant there. Curing needs moisture in the air. |
| Temperature | Apply MS973 from +5°C to +35°C. Below +5°C, wait. |
One 600 ml pack of MS973 covers about 12 metres of a 10×5 mm joint at a 2:1 ratio. That coverage belongs to the universal grade. Ask for the current sheet of MS973-KB before you use the same metre count on a kitchen joint. The price is on the proforma. This page does not print a mould-test result or a certificate number.
中文
湿区分成两种缝。厨卫要 MS973-KB,这个型号的名称是防霉。阳台边缘只有在它属于低位移墙缝时,才按通用型 MS973 来定。两种都不是把整块板面涂一层。不点名客户。
- 密度、表干和拉伸写在 MS973 上,在 MS973-KB 有自己的表之前不要抄过去。
- 低位移墙缝按缝宽深比 2:1。这不是阳台板的防水膜。
- 天然石材先在边角料上做污染测试。
- 要上漆就等固化后上水性漆,并先试涂料。
- 完全密闭处不能用。MS973 的施工温度是 +5°C 到 +35°C。
- 600 ml 的米数属于通用型。厨卫型号先要它自己的现行数据表,再套用米数。本页不写防霉检测值,不印证书编号。价格在形式发票上。